Incoloy Alloy is a kind of nickel based high temperature alloy.
Yesom Group offers Incoloy Alloy in shape of wire, bar, plate, strip, coil, flange, etc.
	Alloy Grade: Incoloy 800 ,  Incoloy 800H ,  Incoloy 800HT ,  Incoloy 825 , Incoloy 925 , Incoloy 926 ,
 
Incoloy A286 , Incoloy 20 , Incoloy 28 , Incoloy 200 , Incoloy 201
	
 
Incoloy 800
| Incoloy 800/800H/800HT (UNS N08800 / UNS N08810 / UNS N08811) | |||
| Chemical Composition % | Ni: 30-35 | Cr: 19-23 | Fe: Margin | 
| Cu: ≤0.75 | Mn: ≤1.5 | Co: ≤2.0 | |
| Ti: 0.15-0.60 | Al: 0.15-0.60 | C: ≤0.1 | |
| Si: ≤1.0 | S: ≤0.015 | ||
| Melting Point ℃ | 1350-1400 | ||
| Density g/cm3 | 8 | ||
| Executive Standards | ASTM: B409 | AMS: 5871 | |
| Application Area | Nitric acid condenser, steam heating tube, heating element tube | ||
				
				 
						Designations: AWS 020
					 
						 
					 
						 
					 
						Alloy Details
					 
						 
					 
						Heat treatment of finished parts
					 
						 
					 
						Properties
					 
						 
					 
					
							
								
					
									 
								
										Density
									 
									
										Melting Point
									 
									
										Coefficient of Expansion
									 
									
										Modulus of Rigidity
									 
									
										Modulus of Elasticity
									 
								
									 
								
										7.94 g/cm³
									 
									
										1385 °C
									 
									
										14.4 μm/m °C (20 – 100 °C)
									 
									
										78.9 kN/mm²
									 
									
										196.5 kN/mm²
									 
								
									 
							
						
										0.287 lb/in³
									 
									
										2525 °F
									 
									
										7.9 x 10-6 in/in °F (70 – 212 °F)
									 
									
										11444 ksi
									 
									
										28500 ksi
									 
								
							
								
					
									 
								
										Condition as supplied by AWI
									 
									
										Type
									 
									
										Temperature
									 
									
										Time
									 
									
										Cooling
									 
								
									 
							
						
										Annealed or Spring Temper
									 
									
										Stress Relieve
									 
									
										450 – 470 °C (840 – 880 °F)
									 
									
										0.5 – 1 Hr
									 
									
										Air
									 
								
							
								
					
									 
								
										Annealed
									 
									
										 
									 
									
										 
									 
								
									 
								
										Approx. tensile strength
									 
									
										<800 N/mm²
									 
									
										<116 ksi
									 
								
									 
							
						
										Approx. operating temperature depending on loading and environment
									 
									
										-200 to +815 °C
									 
									
										-330 to +1500 °C
									 
								
							
								
					
									 
								
										Spring Temper
									 
									
										 
									 
									
										 
									 
								
									 
								
										Approx. tensile strength
									 
									
										800 – 1200 N/mm²
									 
									
										116 – 159 ksi
									 
								
									 
							
						
										Approx. operating temperature depending on loading and environment
									 
									
										-200 to +815 °C
									 
									
										-330 to +1500 °C
									 
								
				
The above information is typical. If you require different please ask.
		
	
	 
 
  
	