Hastelloy Alloy is a kind of nickel based high temperature alloy.
Yesom Group offers Hastelloy Alloy in shape of wire, bar, plate, strip, coil, flange, etc.
	Alloy Grade: Hastelloy C-4 ,  Hastelloy C-22 ,  Hastelloy C-276 , Hastelloy C-2000 , 
                      Hastelloy B , Hastelloy B-2 , Hastelloy B-3 , Hastelloy X
 
	
 
Hastelloy B-3
| Hastelloy B-3 | |||
| Chemical Composition % | Ni: ≥65 | Cr: 1.0-3.0 | Fe: 1.0-3.0 | 
| W: ≤3.0 | Mo: 27-32 | Cu: ≤0.2 | |
| Mn: ≤3.0 | Co: ≤3.0 | Ti: ≤0.2 | |
| Al: ≤0.5 | C: ≤0.01 | Si: ≤0.1 | |
| P: ≤0.03 | S: ≤0.01 | V: ≤0.2 | |
| Melting Point ℃ | 1370-1418 | ||
| Density g/cm3 | 9.22 | ||
| Application Area | 
					 It has extensive applications in the fields of chemistry, petrochemicals, energy manufacturing, and pollution control.  Especially in industries such as sulfuric acid, hydrochloric acid, phosphoric acid, and acetic acid  | 
			||
	
	
	 
			Designations: AWS 051
		 
			 
		 
			Specifications: ASTM B335  ,  ASTM B619
		 
			 
		 
			Alloy Details
		 
			 
		 
			Heat treatment of finished parts
		 
			 
		 
			Properties
		 
			 
		 
		The above information is typical. If you require different please ask.
	
				
					
		
						 
					
							Density
						 
						
							Melting Point
						 
						
							Coefficient of Expansion
						 
						
							Modulus of Rigidity
						 
						
							Modulus of Elasticity
						 
					
						 
					
							9.22 g/cm³
						 
						
							1418 °C
						 
						
							10.6 μm/m °C (20 – 100 °C)
						 
						
							83 kN/mm²
						 
						
							216 kN/mm²
						 
					
						 
				
			
							0.333 lb/in³
						 
						
							2585 °F
						 
						
							5.7 x 10-6 in/in °F (70 – 212 °F)
						 
						
							12038 ksi
						 
						
							31329 ksi
						 
					
				
					
		
						 
					
							Condition as supplied by AWI
						 
						
							Type
						 
						
							Temperature
						 
						
							Time
						 
						
							Cooling
						 
					
						 
				
			
							Annealed or Spring Temper
						 
						
							Stress Relieve
						 
						
							400 – 450 °C (750 – 840 °F)
						 
						
							2 Hr
						 
						
							Air
						 
					
				
					
		
						 
					
							Annealed
						 
						
							 
						 
						
							 
						 
					
						 
					
							Approx. tensile strength
						 
						
							<1200 N/mm²
						 
						
							<174 ksi
						 
					
						 
				
			
							Approx. operating temperature depending on loading and environment
						 
						
							-200 to +400 °C
						 
						
							-330 to +750 °F
						 
					
				
					
		
						 
					
							Spring Temper
						 
						
							 
						 
						
							 
						 
					
						 
					
							Approx. tensile strength
						 
						
							1600 – 2000 N/mm²
						 
						
							232 – 290 ksi
						 
					
						 
				
			
							Approx. operating temperature depending on loading and environment
						 
						
							-200 to +400 °C
						 
						
							-330 to +750 °F
						 
					
	 
 
  
	