Hastelloy Alloy is a kind of nickel based high temperature alloy.
Yesom Group offers Hastelloy Alloy in shape of wire, bar, plate, strip, coil, flange, etc.
	Alloy Grade: Hastelloy C-4 ,  Hastelloy C-22 ,  Hastelloy C-276 , Hastelloy C-2000 , 
                      Hastelloy B , Hastelloy B-2 , Hastelloy B-3 , Hastelloy X
 
	
 
Hastelloy C-200
| Hastelloy C-2000(UNS N06200、W.Nr.2.4675、NS3405、NS345) | |||
| Chemical Composition % | Ni: Margin | Cr: 22-24 | Fe: ≤3.0 | 
| Mo: 15-17 | Cu: 1.3-1.9 | Mn: ≤0.50 | |
| Co: ≤2.0 | Al: ≤0.50 | C: ≤0.01 | |
| Si: ≤0.08 | P: ≤0.025 | S: ≤0.01 | |
| Melting Point ℃ | 1335-1380 | ||
| Density g/cm3 | 8.9 | ||
| Application Area | Used for acetic acid/acetic anhydride, acid leaching, cellophane manufacturing, chlorination systems, complex mixed acids, electrogalvanizing tank rollers, expansion corrugated pipes, flue gas cleaning systems, geothermal wells, incineration cleaning systems, nuclear combustion regeneration, phosphoric acid production, acid cleaning systems, plate heat exchangers, filtration systems, sulfur dioxide cooling towers, sulfonation systems, pipe heat exchangers, welding valves, hydrogen fluoride furnace cleaning, etc. | ||
	
Designations: AWS 055
	
Specifications: ASTM B574 , ASTM B575 , ASTM B619
	
Alloy Details
	
	 
			 
		 
			Heat treatment of finished parts
		 
			 
		 
			Properties
		 
			 
		 
		The above information is typical. If you require different please ask.
	
				
					
		
						 
					
							Density
						 
						
							Melting Point
						 
						
							Coefficient of Expansion
						 
						
							Modulus of Rigidity
						 
						
							Modulus of Elasticity
						 
					
						 
					
							8.5 g/cm³
						 
						
							1399 °C
						 
						
							12.4 μm/m °C (20 – 100 °C)
						 
						
							79 kN/mm²
						 
						
							206 kN/mm²
						 
					
						 
				
			
							0.307 lb/in³
						 
						
							2550 °F
						 
						
							6.9 x 10-6 in/in °F (70 – 212 °F)
						 
						
							11458 ksi
						 
						
							29878 ksi
						 
					
				
					
		
						 
					
							Condition as supplied by AWI
						 
						
							Type
						 
						
							Temperature
						 
						
							Time
						 
						
							Cooling
						 
					
						 
				
			
							Annealed or Spring Temper
						 
						
							Stress Relieve
						 
						
							400 – 450 °C (750 – 840 °F)
						 
						
							2 Hr
						 
						
							Air
						 
					
				
					
		
						 
					
							Annealed
						 
						
							 
						 
						
							 
						 
					
						 
					
							Approx. tensile strength
						 
						
							<1000 N/mm²
						 
						
							<145 ksi
						 
					
						 
				
			
							Approx. operating temperature depending on loading and environment
						 
						
							-200 to +400 °C
						 
						
							-330 to +750 °F
						 
					
				
					
		
						 
					
							Spring Temper
						 
						
							 
						 
						
							 
						 
					
						 
					
							Approx. tensile strength
						 
						
							1300 – 1600 N/mm²
						 
						
							189 – 232 ksi
						 
					
						 
				
			
							Approx. operating temperature depending on loading and environment
						 
						
							-200 to +400 °C
						 
						
							-330 to +750 °F
						 
					
		
	
	
	 
 
  
	